Tel:+8615900357871
Contact Us

China Office:A-4F, Wantone Center, A6, Chaowai St., Chaoyang Dist., Beijing, China.

Tel/Fax:+86-10-85999168

Mobile/Whatsapp: 0086-15900357871

Email: jackywinn@foxmail.com

Skype: petrolsteels

 

Factory Add.1: Cangzhou Economic Development Zone, Cangzhou, Hebei, China.

Tel/Fax:+86-317-5817177

Email:Sales@petrosteels.com

 

Factory Add.2:Beichen Scientific And Technological Zone, Tianjin, China.

Tel/Fax:+86-22-58052277

Email: Sales@petrosteels.com


Best 15-5ph Ams 5659 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods

We are leading manufacturer and stockist of STAINLESS 15-5Ph in China. STAINLESS 15-5Ph Technical Data Sheet Alloy 15-5 is a precipitation hardening alloy exhibiting high strength and hardness with moderate corrosion resistance. Alloy 15-5 is a variant of the older 17-4 and 15-5 was designed to...

We are leading manufacturer and stockist of STAINLESS 15-5Ph in China.

 

STAINLESS 15-5Ph Technical Data Sheet

 

Chemical Composition Limits

Weight%

C

Si

Mn

P+S max

Cr

Ni

Cu

Cb

Fe

Mo

AMS 5659
15-5

0.07

1.0

1.0

0.03P
0.015S

14.0-15.50

3.50-4.50

2.50-4.50

0.45

Bal

0.50

Alloy 15-5 is a precipitation hardening alloy exhibiting high strength and hardness with moderate corrosion resistance. Alloy 15-5 is a variant of the older 17-4 and 15-5 was designed to have greater toughness than S17400, especially in the through-thickness (short transverse) direction. Alloy 15-5 is used in applications that require high transverse strength and toughness such as engine parts, aircraft components, nuclear reactor components etc.

 

STAINLESS 15-5Ph Mechanical Properties

 

Material

Condition

Ultimate Tensile Strength (ksi)

0.2 % Yield Strength (ksi)

Elongation % in 2D

% Reduction of Area

Rockwell C Hardness

Alloy 15-5 PH
Bar AMS 5659

Cond A

-

-

-

-

363 HB max

Alloy 15-5 PH
Bar AMS 5659

H900

190

170

10

35

388-444

Alloy 15-5 PH
Bar AMS 5659

H925

170

155

10

38

375-429

Alloy 15-5 PH
Bar AMS 5659

H1025

155

145

12

45

331-401

Alloy 15-5 PH
Bar AMS 5659

H1075

145

125

13

45

311-375

Alloy 15-5 PH
Bar AMS 5659

H1100

140

115

14

45

302-363

Alloy 15-5 PH
Bar AMS 5659

H1150

135

105

16

50

277-352

 

Material

Condition

Ultimate Tensile Strength (ksi)

0.2 % Yield Strength (ksi)

Elongation % in 2D

% Reduction of Area

Rockwell C Hardness

Alloy 15-5 PH
Sheet/Plate AMS 5862

Cond A

-

-

-

-

38 max

Alloy 15-5 PH
Sheet/Plate AMS 5862

H900

190

170

5

-

40-47

Alloy 15-5 PH
Sheet/Plate AMS 5862

H925

170

155

5

-

38-45

Alloy 15-5 PH
Sheet/Plate AMS 5862

H1025

155

145

5

-

35-42

Alloy 15-5 PH
Sheet/Plate AMS 5862

H1075

145

125

5

-

33-39

Alloy 15-5 PH
Sheet/Plate AMS 5862

H1100

140

115

5

-

32-38

Alloy 15-5 PH
Sheet/Plate AMS 5862

H1150

135

105

8

-

28-37

 

STAINLESS 15-5Ph Specifications
15-5 ESR to the following specifications:
AMS 5659 TYPE 2 
ASTM-A-484
UNS-S15500
 
15-5 PH VAC MELT to the following specifications:
AMS 5659 TYPE 1
ASTM-A-484
 
15-5 VM COND H-1025 to the following specifications
AMS-5659 T-1 (COND H-1025)
AMS-H-6875
ASTM-A-484
ASTM-A-564 TYPE XM-12 (COND H-1025)
 
15-5 VM COND H-1050 to the following specifications
AMS-5659 T-1 (EXC. COND)
AMS-H-6875
ASTM-A-484
ASTM-A-564 TYPE XM-12 (EXC. COND)
BAC-5619 (150-170 MIN. TENS.)
  
AMS 5862 Sheet, Strip and Plate. 
AMS 5826 Welding Wire 
UNS : S15500

STAINLESS MS 5604


The STAINLESS 15-5Ph items which we can manufacture and supply are the followings.

STAINLESS 15-5Ph Rod

STAINLESS 15-5Ph Rings

STAINLESS 15-5Ph Forgings

STAINLESS 15-5Ph pipe

STAINLESS 15-5Ph tube

STAINLESS 15-5Ph bars

STAINLESS 15-5Ph plates

STAINLESS 15-5Ph sheets

STAINLESS 15-5Ph Strip

STAINLESS 15-5Ph wire

STAINLESS 15-5Ph fitting Union

STAINLESS 15-5Ph Pipe Elbows

STAINLESS 15-5Ph PIPE Tee

STAINLESS 15-5Ph ADAPTERS

STAINLESS 15-5Ph pipe bend

STAINLESS 15-5Ph reducers

STAINLESS 15-5Ph fitting caps

STAINLESS 15-5Ph pipe outlets

STAINLESS 15-5Ph Stub Ends

STAINLESS 15-5Ph Couplings

STAINLESS 15-5Ph pipe Nipples

STAINLESS 15-5Ph BUSHINGS

STAINLESS 15-5Ph pipes sockets

STAINLESS 15-5Ph Pipe Gasket

STAINLESS 15-5Ph pipe joints

STAINLESS 15-5Ph pipe Cross

STAINLESS 15-5Ph Pipe Wyes

STAINLESS 15-5Ph seal ring

STAINLESS 15-5Ph Flange

STAINLESS 15-5Ph bolts

STAINLESS 15-5Ph nuts

STAINLESS 17-4Ph

 

ONE OF THE KIND, MILLIONS OF CHOICES

SUPERIOR QUALITY

PROMPT DELIVERY

FAVORABLE FEEDBACK

ALL AVAILABLE IN SMICO

SELECT SMICO, YOU WILL BE RIGHT

 

For more info and price of STAINLESS 15-5Ph, please send us inquiry and you will have quick reply soon. 


Hot Tags: 15-5ph AMS 5862