Excellent 13-8mo Stainless Steel Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods

We are leading manufacturer and stockist of 13-8ph stainless steel in China. 13-8ph stainless steel Technical Data Sheet 13-8 stainless alloy (UNS S13800) is a martensitic precipitation-hardening stainless steel that has excellent strength, high hardness, superior toughness, and good corrosion...

We are leading manufacturer and stockist of 13-8ph stainless steel in China.

 13-8ph stainless steel Technical Data Sheet

13-8ph stainless steel Chemical Composition Limits

Weight%

C

P

Si

Ni

Al

Fe

Mn

S

Cr

Mo

N

13-8 Mo

0.05 max

0.010 max

0.10 max

7.5-8.5

0.90-1.35

Bal

0.10 max

0.008 max

12.25-13.25

2.0-2.5

0.01 max

13-8 stainless alloy (UNS S13800) is a martensitic precipitation-hardening stainless steel that has excellent strength, high hardness, superior toughness, and good corrosion resistance. Compared to other ferrous-base materials alloy 13-8 offers a high level of useful mechanical properties under severe environmental conditions. Alloy 13-8 is used in Aerospace components, landing gear, nuclear reactor components, petrochemical industry, injection molding equipment etc. Alloy 13-8 in the annealed condition can be strengthened further by relatively low temperature heat treatment.

 

13-8ph stainless steel Mechanical Properties

Material

Condition

Ultimate Tensile Strength (ksi)

0.2 % Yield Strength (ksi)

Elongation % in 2D

% Reduction of Area

Rockwell C Hardness

Alloy 13-8
Sheet AMS 5864

Cond A

-

-

-

-

38 max

Alloy 13-8
Sheet AMS 5864

H950

220

205

10

45

45

Alloy 13-8
Sheet AMS 5864

H1000

205

190

10

50

43

Alloy 13-8
Sheet AMS 5864

H1025

185

175

11

50

41

Alloy 13-8
Sheet AMS 5864

H1050

175

165

12

50

40

Alloy 13-8
Sheet AMS 5864

H1100

150

135

14

50

34

Alloy 13-8
Sheet AMS 5864

H1150

135

90

14

50

30

 

Material

Condition

Ultimate Tensile Strength (ksi)

0.2 % Yield Strength (ksi)

Elongation % in 2D

% Reduction of Area

Rockwell C Hardness

Alloy 13-8
Bar AMS 5629

Cond A

-

-

-

-

363 HB Max

Alloy 13-8
Bar AMS 5629

H950

220

205

10

45

45

Alloy 13-8
Bar AMS 5629

H1000

205

190

10

50

43

Alloy 13-8
Bar AMS 5629

H1025

185

175

11

50

41

Alloy 13-8
Bar AMS 5629

H1050

175

165

12

50

40

Alloy 13-8
Bar AMS 5629

H1100

150

135

14

50

34

Alloy 13-8
Bar AMS 5629

H1150

135

90

14

50

30

 

13-8ph stainless steel Specifications

Bar

AMS 5629 Type 1, ASTM A 564 Grade XM13, ASME SA564 Grade XM13, DMS 2100, HMS 6 1105, HMS 6 1105 Exc Sonic, Sonic Per MIL STD 2154 Class A, STO 160 LBO 013 

Plate

AMS 5864, ASTM A 564, ASME SA693

Wire

ASTM A 564, ASME SA564, AMS 5864, AMS 5520

Sheet

ASTM A693, ASME SA693, AMS 5864

Strip

ASTM A693, ASME SA693

Forgings

ASTM A 705, ASME SA705

Rings

13-8 AMS 5629

Extrusions

13-8 AMS 5629

 

 

The 13-8ph stainless steel items which we can manufacture and supply are the followings.

13-8ph stainless steel Rod

13-8ph stainless steel Rings

13-8ph stainless steel Forgings

13-8ph stainless steel pipe

13-8ph stainless steel tube

13-8ph stainless steel bars

13-8ph stainless steel plates

13-8ph stainless steel sheets

13-8ph stainless steel Strip

13-8ph stainless steel wire

13-8ph stainless steel fitting Union

13-8ph stainless steel Pipe Elbows

13-8ph stainless steel PIPE Tee

13-8ph stainless steel ADAPTERS

13-8ph stainless steel pipe bend

13-8ph stainless steel reducers

13-8ph stainless steel fitting caps

13-8ph stainless steel pipe outlets

13-8ph stainless steel Stub Ends

13-8ph stainless steel Couplings

13-8ph stainless steel pipe Nipples

13-8ph stainless steel BUSHINGS

13-8ph stainless steel pipes sockets

13-8ph stainless steel Pipe Gasket

13-8ph stainless steel pipe joints

13-8ph stainless steel pipe Cross

13-8ph stainless steel Pipe Wyes

13-8ph stainless steel seal ring

13-8ph stainless steel Flange

13-8ph stainless steel bolts

13-8ph stainless steel nuts

15-7Mo stainless steel Rod

15-7Mo stainless steel Rings

15-7Mo stainless steel Forgings

15-7Mo stainless steel pipe

15-7Mo stainless steel tube

15-7Mo stainless steel bars

15-7Mo stainless steel plates

15-7Mo stainless steel sheets

15-7Mo stainless steel Strip

15-7Mo stainless steel wire

 

ONE OF THE KIND, MILLIONS OF CHOICES

SUPERIOR QUALITY

PROMPT DELIVERY

FAVORABLE FEEDBACK

ALL AVAILABLE IN SMICO

SELECT SMICO, YOU WILL BE RIGHT

For more info and price of 13-8ph stainless steel, please send us inquiry and you will have quick reply soon.


Hot Tags: Excellent 13-8mo Stainless Steel Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods,Stainless Steel