Tel:+8615900357871
Contact Us

China Office:A-4F, Wantone Center, A6, Chaowai St., Chaoyang Dist., Beijing, China.

Tel/Fax:+86-10-85999168

Mobile/Whatsapp: 0086-15900357871

Email: jackywinn@foxmail.com

Skype: petrolsteels

 

Factory Add.1: Cangzhou Economic Development Zone, Cangzhou, Hebei, China.

Tel/Fax:+86-317-5817177

Email:Sales@petrosteels.com

 

Factory Add.2:Beichen Scientific And Technological Zone, Tianjin, China.

Tel/Fax:+86-22-58052277

Email: Sales@petrosteels.com


Reliable 17-7ph Stainless Steel Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods

We are leading manufacturer and stockist of STAINLESS 17-7Ph in China. STAINLESS 17-7Ph Technical Data Sheet Alloy 17-7 PH a precipitation hardening stainless steel that provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum...

We are leading manufacturer and stockist of STAINLESS 17-7Ph in China.

STAINLESS 17-7Ph Technical Data Sheet 

STAINLESS 17-7Ph Chemical Composition Limits

Weight%

C

Mn

Si

P

S

Cr

Ni

Al

17-7PH

0.09 max

1.00 max

1.00 max

0.040 max

0.030 max

16.00-18.00

6.50-7.75

0.75-1.50

Alloy 17-7 PH a precipitation hardening stainless steel that provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. 

Corrosion Resistance
17-7 PH stainless steel provides corrosion resistance in conditions TH 1050 and RH 950 is generally superior to that of the standard hardenable chromium types of stainless steels such as Types 410, 420 and 431, but is not quite as good as chromium-nickel Type 304. Corrosion resistance in Condition CH 900 approaches that of Type 304 in most environments.
 

STAINLESS 17-7Ph Typical Mechanical Properties

 

Material

Condition

Ultimate Tensile Strength (ksi)

0.2 % Yield Strength (ksi)

Elongation % in 2D

% Reduction of Area

Rockwell C Hardness

17-7 Sheet / Strip
AMS 5528

Cond A

105 max

65

20

-

92 HRB max

17-7 Sheet / Strip
AMS 5528

TH1050

180-120

150

4-6

-

38-46

17-7 Sheet / Strip

RH950

220

200

9

-

46

17-7 Sheet / Strip
AMS 5529

Cond C

200 min

175 min

1

-

41 min

17-7 Sheet / Strip
AMS 5529

CH 900

240 min

230 min

1

-

46 min

17-7 Bar
AMS 5644

Cond A

170 min

140 min

6

25

363 HB min

 

STAINLESS 17-7Ph Specifications
Type 17-7 PH Stainless Steel is covered by the following specifications:
AMS 5528 Sheet, Strip and Plate
AMS 5529 Sheet, Strip Cold Rolled
AMS 5568 Welded Tubing
AMS 5644 Bars and Forgings (Cap. ASTM A 564 Type 631)
AMS 5678 Wire
AMS 5824 Welding Wire
MIL-S-25043 Cond. C, Sheet, Strip and Plate
ASTM A 693, ASTM A 313, ASTM A 564, ASTM A 579 and ASTM A 705
ASME SA 564, SA 693 and SA 705
UNS S17700

 

 

The STAINLESS 17-7Ph items which we can manufacture and supply are the followings.

STAINLESS 17-7Ph Rod

STAINLESS 17-7Ph Rings

STAINLESS 17-7Ph Forgings

STAINLESS 17-7Ph pipe

STAINLESS 17-7Ph tube

STAINLESS 17-7Ph bars

STAINLESS 17-7Ph plates

STAINLESS 17-7Ph sheets

STAINLESS 17-7Ph Strip

STAINLESS 17-7Ph wire

STAINLESS 17-7Ph fitting Union

STAINLESS 17-7Ph Pipe Elbows

STAINLESS 17-7Ph PIPE Tee

STAINLESS 17-7Ph ADAPTERS

STAINLESS 17-7Ph pipe bend

STAINLESS 17-7Ph reducers

STAINLESS 17-7Ph fitting caps

STAINLESS 17-7Ph pipe outlets

STAINLESS 17-7Ph Stub Ends

STAINLESS 17-7Ph Couplings

STAINLESS 17-7Ph pipe Nipples

STAINLESS 17-7Ph BUSHINGS

STAINLESS 17-7Ph pipes sockets

STAINLESS 17-7Ph Pipe Gasket

STAINLESS 17-7Ph pipe joints

STAINLESS 17-7Ph pipe Cross

STAINLESS 17-7Ph Pipe Wyes

STAINLESS 17-7Ph seal ring

STAINLESS 17-7Ph Flange

STAINLESS 17-7Ph bolts

STAINLESS 17-7Ph nuts

 

ONE OF THE KIND, MILLIONS OF CHOICES

SUPERIOR QUALITY

PROMPT DELIVERY

FAVORABLE FEEDBACK

ALL AVAILABLE IN SMICO

SELECT SMICO, YOU WILL BE RIGHT

 

For more info and price of STAINLESS 17-7Ph, please send us inquiry and you will have quick reply soon.


Hot Tags: Reliable 17-7ph Stainless Steel Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods,Stainless Steel