Tel:+86-13436334453
Contact Us

China Office:A-4F, Wantone Center, A6, Chaowai St., Chaoyang Dist., Beijing, China.

Tel/Fax:+86-10-85999168

Mobile/Whatsapp: 0086-13436334453

Email: jackywinn@foxmail.com

Skype: petrolsteels

 

Factory Add.1: Cangzhou Economic Development Zone, Cangzhou, Hebei, China.

Tel/Fax:+86-317-5817177

Email:Sales@petrosteels.com

 

Factory Add.2:Beichen Scientific And Technological Zone, Tianjin, China.

Tel/Fax:+86-22-58052277

Email: Sales@petrosteels.com


Stainless Nitronic 40 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods

We are leading manufacturer and stockist of STAINLESS Nitronic 40 in China. STAINLESS Nitronic 40 Technical Data Sheet Nitronic 40 (21-6-9) is a high-manganese nitrogen strengthened stainless steel. Nitronic 40 properties include high strength in the annealed condition, excellent resistance to...

We are leading manufacturer and stockist of STAINLESS Nitronic 40 in China.

 

STAINLESS Nitronic 40 Technical Data Sheet

STAINLESS Nitronic 40 Chemical Composition Limits

Weight%

C

P

Si

Ni

Fe

Mn

S

Cr

N

Mo

Cu

Nitronic 40 (21-6-9)

0.04 max

0.060 max

1.00 max

5.5-7.5

Bal

8-10

0.030 max

19-21.5

0.15-0.40

0.75 max

0.75 max

 

Nitronic 40 (21-6-9) is a high-manganese nitrogen strengthened stainless steel. Nitronic 40 properties include high strength in the annealed condition, excellent resistance to corrosion at high temperatures, readily weldable and it can also be fabricated. Nitronic 40 is used in a numerous applications including aircraft engine components, chemical processing, pollution control equipment.     

 

STAINLESS Nitronic 40 Mechanical Properties

 

Alloy

Cross Section Size

Test Direction

Yield Strength 0.2%

Ultimate Tensile Strength

Elongation in 2"(%)

Reduction of Area %

Rockwell B Hardness

ksi

MPa

ksi

MPa

Nitronic 40 (21-6-9)

6" (152mm) sq

Longitudinal

62

428

95

655

46

69


Nitronic 40 (21-6-9)

6" (152mm) sq

Transverse

52

358

93

641

30

45


Nitronic 40 (21-6-9)

4" (102mm) sq

Longitudinal

56

386

97

668

53

73


Nitronic 40 (21-6-9)

1" (25.4mm)sq

Longitudinal

52

358

101

696

53

73

90

 

STAINLESS Nitronic 40 Specifications

AMS 5656 Bar / Wire

AMS 5595 Sheet / Plate / Strip

AMS 5561 Welded tube

AMS 5562 Seamless Tube

AMS 5656 Rings / Extrusions

MIL-T-9821

ASTM A276 / ASME SA276

ASTM A412 / ASME SA412

ASTM A580 / ASME SA580

UNS S21906

 

 

The STAINLESS Nitronic 40 items which we can manufacture and supply are the followings.

STAINLESS Nitronic 40 Rod

STAINLESS Nitronic 40 Rings

STAINLESS Nitronic 40 Forgings

STAINLESS Nitronic 40 pipe

STAINLESS Nitronic 40 tube

STAINLESS Nitronic 40 bars

STAINLESS Nitronic 40 plates

STAINLESS Nitronic 40 sheets

STAINLESS Nitronic 40 Strip

STAINLESS Nitronic 40 wire

STAINLESS Nitronic 40 fitting Union

STAINLESS Nitronic 40 Pipe Elbows

STAINLESS Nitronic 40 PIPE Tee

STAINLESS Nitronic 40 ADAPTERS

STAINLESS Nitronic 40 pipe bend

STAINLESS Nitronic 40 reducers

STAINLESS Nitronic 40 fitting caps

STAINLESS Nitronic 40 pipe outlets

STAINLESS Nitronic 40 Stub Ends

STAINLESS Nitronic 40 Couplings

STAINLESS Nitronic 40 pipe Nipples

STAINLESS Nitronic 40 BUSHINGS

STAINLESS Nitronic 40 pipes sockets

STAINLESS Nitronic 40 Pipe Gasket

STAINLESS Nitronic 40 pipe joints

STAINLESS Nitronic 40 pipe Cross

STAINLESS Nitronic 40 Pipe Wyes

STAINLESS Nitronic 40 seal ring

STAINLESS Nitronic 40 Flange

STAINLESS Nitronic 40 bolts

STAINLESS Nitronic 40 nuts

 

ONE OF THE KIND, MILLIONS OF CHOICES

SUPERIOR QUALITY

PROMPT DELIVERY

FAVORABLE FEEDBACK

ALL AVAILABLE IN SMICO

SELECT SMICO, YOU WILL BE RIGHT

 

For more info and price of STAINLESS Nitronic 40, please send us inquiry and you will have quick reply soon.