Trustable Stainless 410 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods Printing Spherical Powder

We are leading manufacturer and stockist of STAINLESS 410 in China. Technical Data Sheet of STAINLESS 410 Type 410 is a basic hardenable martensitic stainless steel and is well suited for use in highly stressed parts where properties such as corrosion resistance, good strength and ductility are...

We are leading manufacturer and stockist of STAINLESS 410 in China.

 

Technical Data Sheet of STAINLESS 410

 

Chemical Composition Limits of STAINLESS 410

Weight%

C

Si

Mn

P

S

Cr

Fe

Alloy 410

0.15 max

1.0 max

1.0 max

0.040 max

0.030 max

11.5-13.5

Bal

Type 410 is a basic hardenable martensitic stainless steel and is well suited for use in highly stressed parts where properties such as corrosion resistance, good strength and ductility are required. 410 is used for steam / gas turbine blades and buckets, bushings, valve components, fasteners, nuclear reactor control rod mechanisms, petrochemical equipment and machine parts.

 

Typical Mechanical Properties of STAINLESS 410

 

Material

Tempering Temp °C (°F)

0.2 % Yield Strength (Mpa)

Ultimate Tensile Strength (Mpa)

% Elongation in 2"

% Reduction of Area

Charpy V Notch Impact Strength (J)

Hardness Brinell

Alloy 410 Bar
Hardened 1850°F (1010°C) 30 mins, oil quench, tempered 4 Hrs

260 (500)

1089

1331

17

62

76

401

Alloy 410 Bar
Hardened 1850°F (1010°C) 30 mins, oil quench, tempered 4 Hrs

317 (700)

1069

1296

17

60

66

401

Alloy 410 Bar
Hardened 1850°F (1010°C) 30 mins, oil quench, tempered 4 Hrs

482 (900)

1014

1303

18

58

38

401

Alloy 410 Bar
Hardened 1850°F (1010°C) 30 mins, oil quench, tempered 4 Hrs

538 (1000)

917

965

19

62

33

285

Alloy 410 Bar
Hardened 1850°F (1010°C) 30 mins, oil quench, tempered 4 Hrs

593 (1100)

724

827

20

63

52

248

Alloy 410 Bar
Hardened 1850°F (1010°C) 30 mins, oil quench, tempered 4 Hrs

649 (1200)

634

731

21

65

119

223


STAINLESS 410 Steel is covered by the following specifications:
AMS 5504 Sheet / strip / plate
AMS 5505 Sheet / strip / plate (Mod)
AMS 5591 Seamless tube
AMS 5609 Bars / wire
AMS 5611 Bars / wire / forging
AMS 5612 (51410 Modified) Bar, Wire, Forgings, Tubing and Rings
AMS 5613 Bars / wire / forging
AMS 5614 Bars / wire / forging
QQ-S-763
QQ-S-766
ASTM A176 / ASME SA176
ASTM A240 / ASME SA240
ASTM A276 / ASME SA276
ASTM A479 / ASME A479
ASTM A493 / ASME SA493
ASTM A580 / ASME SA580
ASTM F899
UNS S41000

 

 

The STAINLESS 410 items which we can manufacture and supply are the followings.

STAINLESS 416

STAINLESS 410 Rod

STAINLESS 410 Rings

STAINLESS 410 Forgings

STAINLESS 410 pipe

STAINLESS 410 tube

STAINLESS 410 bars

STAINLESS 410 plates

STAINLESS 410 sheets

STAINLESS 410 Strip

STAINLESS 410 wire

STAINLESS 410 fitting Union

STAINLESS 410 Pipe Elbows

STAINLESS 410 PIPE Tee

STAINLESS 410 ADAPTERS

STAINLESS 410 pipe bend

STAINLESS 410 reducers

STAINLESS 410 fitting caps

STAINLESS 410 pipe outlets

STAINLESS 410 Stub Ends

STAINLESS 410 Couplings

STAINLESS 410 pipe Nipples

STAINLESS 410 BUSHINGS

STAINLESS 410 pipes sockets

STAINLESS 410 Pipe Gasket

STAINLESS 410 pipe joints

STAINLESS 410 pipe Cross

STAINLESS 410 Pipe Wyes

STAINLESS 410 seal ring

STAINLESS 410 Flange

STAINLESS 410 bolts

STAINLESS 410 nuts

STAINLESS 416 Rod

STAINLESS 416 Rings

STAINLESS 416 Forgings

STAINLESS 416 pipe

STAINLESS 416 tube

STAINLESS 416 bars

STAINLESS 416 plates

STAINLESS 416 sheets

STAINLESS 416 Strip

STAINLESS 416 wire

 

ONE OF THE KIND, MILLIONS OF CHOICES

SUPERIOR QUALITY

PROMPT DELIVERY

FAVORABLE FEEDBACK

ALL AVAILABLE IN SMICO

SELECT SMICO, YOU WILL BE RIGHT

 

For more info and price of STAINLESS 410, please send us inquiry and you will have quick reply soon.


Hot Tags: Trustable Stainless 410 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods Printing Spherical Powder,Stainless Steel