3d Printing Spherical Powder Haynes 25 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods

We are leading manufacturer and stockist of Haynes 25 in China. Haynes 25 Technical Data Sheet Udimet Alloy L-605 / Haynes 25 is a solid solution strengthened cobalt-chromium-tungsten nickel alloy which combines excellent high temperature strength and oxidation resistance to 2000°F with good...

We are leading manufacturer and stockist of Haynes 25 in China.

 

Haynes 25 Technical Data Sheet

Haynes 25 Chemical Composition Limits

Weight%

C

P

Si

Ni

W

Mn

S

Cr

Co

Fe

Alloy L-605

0.05 - 0.15

0.040 max

0.40 max

9.0 - 11.0

14.0 - 16.0

1.0 - 2.0

0.030 max

19.0 - 21.0

Bal

3.0 max

Udimet Alloy L-605 / Haynes 25 is a solid solution strengthened cobalt-chromium-tungsten nickel alloy which combines excellent high temperature strength and oxidation resistance to 2000°F with good resistance to sulfidation, wear and galling. Alloy L-605 / Haynes 25 has good forming characteristics and is capable of being forged, hot worked or cold worked, althoug it does work-harden very rapidly so frequent intermediate annealing treatments are recommend for complex forming operations. Alloy 25 / L-605 can also be readily welded by most conventional welding methods using similar composition welding wire (AMS 5796) or coated electrodes (AMS 5797). Alloy L-605 / Haynes 25 is supplied solution heat treated in the range of 2150-2250°F and rapid air or water quenched to attain optimum properties. Alloy L-605 / Haynes 25 has many applications in military and commercial gas turbine engine components such as rings, blades and combustion chamber parts although for many modern engines it has largely been replaced by Alloy 188 or Alloy 230.

Haynes 25 Mechanical Properties

Material

Temperature °F

Yield Strength 0.2%

Tensile Strength

Elongation (%)

Hardness HB

Extruded Bar
Alloy 25 / L-605

RT

310 Mpa
45 KSI

862 Mpa
125 KSI

30

277 max

 

Material 
Sheet

Thickness (inches)

Yield Strength 0.2%
KSI

Tensile Strength
KSI min 

Elongation (%)

Hardness HRC

Alloy 25 / L-605
Solution Treated (AMS 5537)

0.005-0.020

55-80

130

30

-

Alloy 25 / L-605
Solution Treated (AMS 5537)

0.020-0.032

55-80

130

35

-

Alloy 25 / L-605
Solution Treated (AMS 5537)

0.032-0.043

55-80

130

40

-

Alloy 25 / L-605
Solution Treated (AMS 5537)

0.043-0225

55-80

130

45

-

Haynes 25 Specifications
UNS R30605
AMS 5507 Sheet Strip and Plate 
AMS 5759 Bar and Forging Stock
AMS 5796 Welding Wire
AMS 5797 (UNS W73605) Welding Rod
ASTM F90 Bar and Wire (surgical implant quality)
GE B50T26
GE B50A460 
Tradenames: Udimet Alloy L-605, Haynes 25, Nickelvac L-605 

 

The Haynes 25 items which we can manufacture and supply are the followings.

Haynes 25 Rod

3D printing spherical powder Haynes 25

Haynes 25 Rings

Haynes 25 Forgings

Haynes 25 pipe

Haynes 25 tube

Haynes 25 bars

Haynes 25 plates

Haynes 25 sheets

Haynes 25 Strip

Haynes 25 wire

Haynes 25 fitting Union

Haynes 25 Pipe Elbows

Haynes 25 PIPE Tee

Haynes 25 ADAPTERS

Haynes 25 pipe bend

Haynes 25 reducers

Haynes 25 fitting caps

Haynes 25 pipe outlets

Haynes 25 Stub Ends

Haynes 25 Couplings

Haynes 25 pipe Nipples

Haynes 25 BUSHINGS

Haynes 25 pipes sockets

Haynes 25 Pipe Gasket

Haynes 25 pipe joints

Haynes 25 pipe Cross

Haynes 25 Pipe Wyes

Haynes 25 seal ring

Haynes 25 Flange

Haynes 25 bolts

Haynes 25 nuts

 

ONE OF THE KIND, MILLIONS OF CHOICES

SUPERIOR QUALITY

PROMPT DELIVERY

FAVORABLE FEEDBACK

ALL AVAILABLE IN SMICO

SELECT SMICO, YOU WILL BE RIGHT

 