3d Printing Spherical Powder Waspaloy Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods

3d Printing Spherical Powder Waspaloy Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods

We are leading manufacturer and stockist of Waspaloy in China. Waspaloy Technical Data Sheet WASPALOY is a nickel based age hardenable alloy that possesses high temperature strength while still having a good corrosion resistance, especially to oxidation. WASPALOY can be used at temperatures up...

We are leading manufacturer and stockist of Waspaloy in China.

 

Waspaloy Technical Data Sheet

Waspaloy Chemical Composition Limits



Weight %

Cr

B

Zr

Al

Ti

Mo

Co

Cu

Fe

S

Si

Mn

C

P

Ni

Waspaloy

18-21

0.003-00.1

0.02-0.12

1.2-1.6

2.75-3.25

3.5-5.0

12-15

0.50 max

2 max

0.030 max

0.75 max

1 max

0.02-0.10 max

0.030 max

Bal

WASPALOY is a nickel based age hardenable alloy that possesses high temperature strength while still having a good corrosion resistance, especially to oxidation. WASPALOY can be used at temperatures up to 650°C (1200°F) which is critical rotating applications. WASPALOY is used in gas turbine engine components, missile systems, shafts, spacers, seals, rings, casings, fasteners and many other uses in engine hardware, airframe assemblies.

 

WaspaloyMechanical Properties

Material

Condtion

Thickness

Temp

Tensile Strength ksi

Yield Strength ksi

Elongation in 4D

Hardness HRC

Sheet

Sol Treated, Stabilization + Precipitation HT

0-0.020"

Room

170

110

15

34-44

Sheet

Sol Treated, Stabilization + Precipitation HT

0-0.020"

1000°F

145

100

13


Sheet

Sol Treated, Stabilization + Precipitation HT

over 0.020"

Room

175

115

20

34-44

Sheet

Sol Treated, Stabilization + Precipitation HT

over 0.020"

1000°F

150

105

15


Waspaloy Properties as per AMS 5544. Heat Treatment is as follows:
Annealing 1975°F / 30 mins and Air Cool
Solution Heat Treatment 1825°F / 2hrs and Air Cool
Stabilization Heat Treatment 1550°F /4hrs and Air Cool
Precipitation Heat Treatment 1400°F / 16 hrs and Air Cool

Waspaloy Bar Properties
Properties as per AMS 5708 type 2 (capable of AMS 5709) Heat Treatment is as follows
Solution Treat 1900 - 1975°F / 1-4 hours and Air Cool
Resulting hardness not higher than 302HB
Stabilization Heat Treatment Heat to 1550°F / 4 hrs and Air Cool
Precipitaion Heat Treatment Heat to 1400°F / 16 hrs and Air Cool
Resulting hardness 32-42 HRC

 

Waspaloy Specifications
Rod, Bar, Wire and Forging Stock
ASTM B 637, ISO 9723, ISO 9724, ISO 9725, AMS 5704, AMS 5706, AMS 5707, AMS 5708, AMS 5709, AMS 5828, MAM 5706, AECMA PrEN 2193, AECMA PrEN 2194, AECMA PrEN 2406, AECMA PrEN 2958, AECMA PrEN 2959, AECMA PrEN 2960, AECMA PrEN 3220.

Plate, Sheet and Strip
AMS 5544, AECMA PrEN 2195
UNS N07001, W. Nr 2.4654, MSRR 7192

Multimet N155

AMS 5532 Sheet, Plate and Strip

AMS 5769 Bars, Rings and Forgings

AMS 5794 Welding Wire

AMS 5795 Coated Electrodes

UNS R30155


The Waspaloy items which we can manufacture and supply are the followings.

Waspaloy Rod

3D printing spherical powder Waspaloy

Waspaloy Rings

Waspaloy Forgings

Waspaloy pipe

Waspaloy tube

Waspaloy bars

Waspaloy plates

Waspaloy sheets

Waspaloy Strip

Waspaloy wire

Waspaloy fitting Union

Waspaloy Pipe Elbows

Waspaloy PIPE Tee

Waspaloy ADAPTERS

Waspaloy pipe bend

Waspaloy reducers

Waspaloy fitting caps

Waspaloy pipe outlets

Waspaloy Stub Ends

Waspaloy Couplings

Waspaloy pipe Nipples

Waspaloy BUSHINGS

Waspaloy pipes sockets

Waspaloy Pipe Gasket

Waspaloy pipe joints

Waspaloy pipe Cross

Waspaloy Pipe Wyes

Waspaloy seal ring

Waspaloy Flange

Waspaloy bolts

Waspaloy nuts

 

ONE OF THE KIND, MILLIONS OF CHOICES

SUPERIOR QUALITY

PROMPT DELIVERY

FAVORABLE FEEDBACK

ALL AVAILABLE IN SMICO

SELECT SMICO, YOU WILL BE RIGHT

 

For more info and price of Waspaloy, please send us inquiry and you will have quick reply soon. 