Email: Sales@petrosteels.com


Excellent 3d Printing Spherical Powder Rene 41 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods

We are leading manufacturer and stockiest of Rene 41 in China. Rene 41 Technical Data Sheet Rene 41 is an age hardening nickel base super alloy with has exceptional strength from room temperature through to between 650°C - 980°C (1200 - 1800ºF). R 41 is designed for use in severely stressed high...

We are leading manufacturer and stockiest of Rene 41 in China.

Rene 41 Technical Data Sheet

Rene 41 Chemical Composition Limits

Weight %

C

Si

Ni

Co

Al

Fe

Mn

Cr

Mo

Ti

B

R41
Rene 41

0.06 - 0.12

0.20 max

Bal

10-12

1.4-1.6

5.0 max

0.10 max

18-20

9.0-10.50

3-3.30

0.003-0.010

Rene 41 is an age hardening nickel base super alloy with has exceptional strength from room temperature through to between 650°C - 980°C (1200 - 1800ºF). R 41 is designed for use in severely stressed high temperature applications. Rene 41 is typically used in hot components for jet engines, rocket engines, turbine blades, turbine wheels, torque rings, bolting, springs and much more.

 

Rene 41 Mechanical Properties

Material

Tensile Strength ksi

Yield Strength ksi

Elongation in 4D

Reduction of Area

Hardness

Rene 41 (R41)
Solution Treated Bar





363 HB max

Rene 41 (R41)
Solution Treated Aged Bar 

170

130

8

10

311 HB min

Rene 41 (R41)
Solution Treated Sheet

170 max

100 max

30 max


30HRC max

Rene 41 (R41)
Solution Treated Aged Sheet

170 min

130 min

10 min


35 HRC min

 

Rene 41 Specifications
UNS N07041
Werkstoff Nr. 2.4973
AISI 683
SAE AMS 5712 Bar
SAE AMS 5545 Sheet, Strip and Plate
GE B50T59 Sheet, Plate, Strip, Bars and Forgings
GE B50TF76C Sheet, Plate, Strip
GE B50TF109C Sheet, Strip, Plate, Solution Treated
SAE AMS 5713 Bar (VAC MELT)
SAE AMS 5800 Welding Wire
MSRR 9500/241 Welding Wire
Tradenames - Rene 41, Pyromet Alloy 41 

 

 

The Rene 41 items which we can manufacture and supply are the followings.

Rene 41 Rod

3D printing spherical powder Rene 41

Rene 41 Rings

Rene 41 Forgings

Rene 41 pipe

Rene 41 tube

Rene 41 bars

Rene 41 plates

Rene 41 sheets

Rene 41 Strip

Rene 41 wire

Rene 41 fitting Union

Rene 41 Pipe Elbows

Rene 41 PIPE Tee

Rene 41 ADAPTERS

Rene 41 pipe bend

Rene 41 reducers

Rene 41 fitting caps

Rene 41 pipe outlets

Rene 41 Stub Ends

Rene 41 Couplings

Rene 41 pipe Nipples

Rene 41 BUSHINGS

Rene 41 pipes sockets

Rene 41 Pipe Gasket

Rene 41 pipe joints

Rene 41 pipe Cross

Rene 41 Pipe Wyes

Rene 41 seal ring

Rene 41 Flange

Rene 41 bolts

Rene 41 nuts

Cobalt Alloy 6b

Stellite 6b

AMS 5894 bar

AMS 5894 sheet

AMS 5894 plate

UNS R30016

 

ONE OF THE KIND, MILLIONS OF CHOICES

SUPERIOR QUALITY

PROMPT DELIVERY

FAVORABLE FEEDBACK

ALL AVAILABLE IN SMICO

SELECT SMICO, YOU WILL BE RIGHT

 

For more info and price of Rene 41, please send us inquiry and you will have quick reply soon.


Hot Tags: Excellent 3d Printing Spherical Powder Rene 41 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods,Superalloys