Premium 3D Printing Spherical Powder Nimonic 75 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods

We are leading manufacturer and stockist of Nimonic 75 in China. Nimonic 75 Technical Data Sheet Nimonic 75 (UNS N06075, Nimonic 75) is a 80/20 nickel-chromium alloy with controlled additions of titanium and carbon. Nimonic 75 has good mechanical properties and oxidation resistance at high...

We are leading manufacturer and stockist of Nimonic 75 in China.

Nimonic 75 Technical Data Sheet

Nimonic 75 Chemical Composition Limits

Weight%

Ni

Cr

Ti

C

Si

Cu

Fe

Mn

Alloy 75
Nimonic 75

Bal

18.9 - 21.0

0.2 / 0.6

0.08 / 0.15

1.0 max

0.5 max

5.0 max

1.0 max

Nimonic 75 (UNS N06075, Nimonic 75) is a 80/20 nickel-chromium alloy with controlled additions of titanium and carbon. Nimonic 75 has good mechanical properties and oxidation resistance at high temperatures. Nimonic 75 is most commonly used for sheet metal fabrications which require oxidation and scaling resistance together with medium strength at high operating temperatures. Nimonic 75 (Nimonic 75) is also used in gas turbine engines, for components of industrial furnaces, for heat treating equipment and fixtures, and in nuclear engineering.

 

 

Nimonic 75 Mechanical Properties

Material

Test Temp °F

Ultimate Tensile Strength (ksi)

0.2 % Yield Strength (ksi)

Elongation in 2"

Alloy 75 Sheet 1925°F Anneal

Room

114.4

59.4

31

Alloy 75 Sheet 1925°F Anneal

1000

105.6

51.9

27

Alloy 75 Sheet 1925°F Anneal

1200

69.3

40.0

32

Alloy 75 Sheet 1925°F Anneal

1400

41.4

22.0

75

Alloy 75 Sheet 1925°F Anneal

1600

20.2

9.9

90

Alloy 75 Sheet 1925°F Anneal

1800

9.7

4.4

91

 

Nimonic 75 Specifications

Rod, Bar, Wire and Forging Stock

BS HR 5, BS HR 504, DIN 17752, AECMA PrEN2306, AECMA PrEN2307, AECMA PrEN2306, AECMA Pr EN2307, AECMA PrEN2402, ISO 9723, ISO 9724, ISO 9725, MSRR 7004

Plate, Sheet, Strip

BS HR 203, DIN 17750, AECMA PrEN2293, AECMA PrEN2302, AECMA PrEN2411, ISO 6208, MSRR 7104

Pipe and Tube

BS HR 403, DIN 17751, AECMA PrEN2294, ISO 6207

Other

DIN 17742, AECMA PrEN2308, Werkstoff Nr 2.4630, W. Nr 2.4951, UNS N06075, Nimonic 75 (tradename), MSRR 7104 and MSRR 7004, AFNOR NC 20T

 

The Nimonic 75 items which we can manufacture and supply are the followings.

Nimonic 75 Rod

3D printing spherical powder Nimonic 75

Nimonic 75 Rings

Nimonic 75 Forgings

Nimonic 75 pipe

Nimonic 75 tube

Nimonic 75 bars

Nimonic 75 plates

Nimonic 75 sheets

Nimonic 75 Strip

Nimonic 75 wire

Nimonic 75 fitting Union

Nimonic 75 Pipe Elbows

Nimonic 75 PIPE Tee

Nimonic 75 ADAPTERS

Nimonic 75 pipe bend

Nimonic 75 reducers

Nimonic 75 fitting caps

Nimonic 75 pipe outlets

Nimonic 75 Stub Ends

Nimonic 75 Couplings

Nimonic 75 pipe Nipples

Nimonic 75 BUSHINGS

Nimonic 75 pipes sockets

Nimonic 75 Pipe Gasket

Nimonic 75 pipe joints

Nimonic 75 pipe Cross

Nimonic 75 Pipe Wyes

Nimonic 75 seal ring

Nimonic 75 Flange

Nimonic 75 bolts

Nimonic 75 nuts

 

ONE OF THE KIND, MILLIONS OF CHOICES

SUPERIOR QUALITY

PROMPT DELIVERY

FAVORABLE FEEDBACK

ALL AVAILABLE IN SMICO

SELECT SMICO, YOU WILL BE RIGHT

 

For more info and price of Nimonic 75, please send us inquiry and you will have quick reply soon.