Qualified 3d Printing Spherical Powder Inconel C276 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods

We are leading manufacturer and stockist of Inconel C276 in China. Inconel C276 Technical Data Sheet Nickel Superalloy C276 is a nickel molybdenum chromium tungsten alloy with the addition of Tungsten. C276 has good fabricability and impressive corrosion resistance in some of the most severe...

We are leading manufacturer and stockist of Inconel C276 in China.

 

Inconel C276 Technical Data Sheet

 

Inconel C276 Chemical Composition Limits

Weight%

C

P

Si

Ni

Co

W

Mn

S

Cr

Mo

V

Fe

C276

0.01 max

0.040 max

0.08 max

Bal

2.5 max

3-4.5

1.00 max

0.030 max

14.5-16.5

15-17

0.35 max

4-7

Nickel Superalloy C276 is a nickel molybdenum chromium tungsten alloy with the addition of Tungsten. C276 has good fabricability and impressive corrosion resistance in some of the most severe environments. Due to C 276's properties it is commonly used in pollution control, chemical, petrochemical and waste incineration applications.

 

 

Inconel C276 Mechanical Properties

Material

Ultimate Tensile (min)

Yield Strength (Min)

Elongation %

Hardness Rb

Ksi

Mpa

Ksi

Mpa

C276 Tube

105.4

727

45.4

313

70

92

C276 Plate

107.4

741

50.3

347

67

89

C276 Bar

110.0

758

52.6

363

62

88

C276 Sheet

115.5

796

54.6

376

60

86

Inconel C276 Specifications
UNS N10276
AMS 5750 Bar, Forgings
WS 2.4819 
ASTM B574, ASME SB574 Bar Products 
ASTM B575, ASME SB575 Plate, Sheet and Strip
ASTM B619, ASME SB619 Welded Pipe
ASTM B622, ASME SB622 Seamless Tubing
ASTM B626, ASME SB 626 Welded Tubing
ASTM B366, ASME SB 366 Wrought Corrosion Resistant Fittings CR HC 276, Wrought ANSI Pressure Fitting-WPHC276
ASTM B564 Forgings
AWS A 5.14, ASME SA 5.14 Welding Wire (ER NiCrMo-4)
AWS A 5.11, ASME SA 5.11 Covered Electrodes (E NiCRMo-4)
NACE MR-01-75
Inconel C276 (trademark)

Similar Specifications
AMS 5750 (Hastelloy C, UNS N10002)
ASTM B751
Werkstoff Nr. 2.4819
DIN 17744, DIN 17750, DIN 17751 and DIN 17752,VRC276

 

 

The Inconel C276 items which we can manufacture and supply are the followings.

Inconel C276 Rod

3D printing spherical powder Incoloy C276

Inconel C276 Rings

Inconel C276 Forgings

Inconel C276 pipe

Inconel C276 tube

Inconel C276 bars

Inconel C276 plates

Inconel C276 sheets

Inconel C276 Strip

Inconel C276 wire

Inconel C276 fitting Union

Inconel C276 Pipe Elbows

Inconel C276 PIPE Tee

Inconel C276 ADAPTERS

Inconel C276 pipe bend

Inconel C276 reducers

Inconel C276 fitting caps

Inconel C276 pipe outlets

Inconel C276 Stub Ends

Inconel C276 Couplings

Inconel C276 pipe Nipples

Inconel C276 BUSHINGS

Inconel C276 pipes sockets

Inconel C276 Pipe Gasket

Inconel C276 pipe joints

Inconel C276 pipe Cross

Inconel C276 Pipe Wyes

Inconel C276 seal ring

Inconel C276 Flange

Inconel C276 bolts

Inconel C276 nuts

 

ONE OF THE KIND, MILLIONS OF CHOICES

SUPERIOR QUALITY

PROMPT DELIVERY

FAVORABLE FEEDBACK

ALL AVAILABLE IN SMICO

SELECT SMICO, YOU WILL BE RIGHT

 

For more info and price of Inconel C276 , please send us inquiry and you will have quick reply soon.


Hot Tags: Qualified 3d Printing Spherical Powder Inconel C276 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods,Superalloys