Tel:+8615900357871
Contact Us

China Office:A-4F, Wantone Center, A6, Chaowai St., Chaoyang Dist., Beijing, China.

Tel/Fax:+86-10-85999168

Mobile/Whatsapp: 0086-15900357871

Email: jackywinn@foxmail.com

Skype: petrolsteels

 

Factory Add.1: Cangzhou Economic Development Zone, Cangzhou, Hebei, China.

Tel/Fax:+86-317-5817177

Email:Sales@petrosteels.com

 

Factory Add.2:Beichen Scientific And Technological Zone, Tianjin, China.

Tel/Fax:+86-22-58052277

Email: Sales@petrosteels.com


Superior Inconel 718 3d Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods

We are leading manufacturer and stockiest of Inconel 718 in China. Technical Data Sheet Inconel 718 (UNS N07718, W Nr 2.4668) is an austenitic nickel-based superalloy. Alloy 718 exhibits excellent high yield tensile and creep-rupture properties at temperatures up to 1300ºF and oxidation...

We are leading manufacturer and stockiest of Inconel 718 in China.

Technical Data Sheet

 

Inconel 718 Chemical Composition Limits

Weight %

C

Mn

P

S

Si

Cr

Ni

Mo

Cb

Ta

Ti

Al

Co

B

Cu

Fe

Alloy 718
AMS 5662

0.08

0.35

0.015

0.015

0.35

17-21

50-55

2.8-3.30

4.75-5.50

0.05

0.65-1.15

0.20-0.80

1.00

0.006

0.30

Rem

Inconel 718 (UNS N07718, W Nr 2.4668) is an austenitic nickel-based superalloy. Alloy 718 exhibits excellent high yield tensile and creep-rupture properties at temperatures up to 1300ºF and oxidation resistance to 1800ºF. Alloy 718 is used in applications that require high strength such as parts for jet engines and high speed airframe parts such as wheels, buckets, spacers and high temperature bolts and fasteners.

This is the preferred treatment in tensile-limited applications as it produces the best transverse ductility in heavy sections, impact strength and low temperature notch tensile strength. However, this treatment has a tendency to produce notch brittleness in stress rupture.

">

Material

Condition

Tensile Strength
ksi

Yield Strength
ksi

Elongation
4D

Reduction of Area
%

Hardness

AMS 5662 Bar

1700-1850°F Anneal

-

-

-

-

≤ 277 HB

AMS 5663 Bar

1700-1850°F Anneal + Age

185

150

12

15

≥331 HB

AMS 5664 Bar

1900-1950°F Anneal

-

-

-

-

3" dia 248 HB
3-5" dia 285 HB

1900-1950°F Anneal + Age

180

150

10

12

≥341 HB

Typical Mechanical Properties of Inconel 718 Bar above and Alloy 718 Sheet below.

Material

Condition

Tensile Strength
ksi

Yield Strength
ksi

Elongation
4D

Hardness

Alloy 718 Sheet

AMS 5596 < 0.1874" thick

140

80

30

102 HRB

Alloy 718 Sheet

AMS 5596 Aged < 0.1874" thick

180

150

12

≥36 HRC

Alloy 718 Sheet

AMS 5597

140

75

30

≤ 25 HRC

Alloy 718 Sheet

AMS 5597 + Aged

180

150

15

≥38 HRC

Availability

Inconel 718 (UNS N07718) is available in Wire, Billet, Strip, Rod, Sheet, Plate, Forging Stock and Welding Wire. For all stock availability contact Sales.

Specifications

UNS N07718

Werkstoff Nr 2.4668

AMS 5596 Sheet, Strip and Plate

AMS 5597 Sheet, Strip and Plate

ASTM B637 Forgings

ASTM B670 Plate, Sheet and Strip

AFNOR NC 19 Fe Nb,

MSRR 7115 and MSRR 7116

Inconel 718 (trademark)

FMC Spec M40110, M40118, M40125, M40902, M40908, M40909, M40910

NACE MR-0175/ISO 15156

 

 

The Inconel 718 items which we can manufacture and supply are the followings.

Inconel 718 Rod

3D printing spherical powder Inconel 718

Inconel 718 Rings

Inconel 718 Forgings

Inconel 718 pipe

Inconel 718 tube

Inconel 718 bars

Inconel 718 plates

Inconel 718 sheets

Inconel 718 Strip

Inconel 718 wire

Inconel 718 fitting Union

Inconel 718 Pipe Elbows

Inconel 718 PIPE Tee

Inconel 718 ADAPTERS

Inconel 718 pipe bend

Inconel 718 reducers

Inconel 718 fitting caps

Inconel 718 pipe outlets

Inconel 718 Stub Ends

Inconel 718 Couplings

Inconel 718 pipe Nipples

Inconel 718 BUSHINGS

Inconel 718 pipes sockets

Inconel 718 Pipe Gasket

Inconel 718 pipe joints

Inconel 718 pipe Cross

Inconel 718 Pipe Wyes

Inconel 718 seal ring

Inconel 718 Flange

Inconel 718 bolts

Inconel 718 nuts

 

 

ONE OF THE KIND, MILLIONS OF CHOICES

SUPERIOR QUALITY

PROMPT DELIVERY

FAVORABLE FEEDBACK

ALL AVAILABLE IN SMICO

SELECT SMICO, YOU WILL BE RIGHT

 

For more info and price of Inconel 718, please send us inquiry and you will have quick reply soon.


Hot Tags: Superior Inconel 718 3d Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods,Superalloys